Here are a few of my most used electrolysis vats. Re-bar seems to work just fine for me, I am not restoring gold or sunken pirates treasure. Just my own treasures. I have not seen pitting, staining, or anything else bad.
I drilled a small hole on each side of the re-bar, wrapped the copper wire around the re-bar. This also help hold the re-bar in place.
Don’t pay attention to my cable colors. Positive on the outside re-bar, negative on the part.
I use this one for medium size objects.
Action Shot:
Small Parts Version:
Action Shot:
And my last entry. I use this one to do the long objects. Primarily Shop Smith Way tubes
Action Shot, I made some modifications to the re-bar, but it is the same vat.